PRODUCT CENTER
CONTACTS
If you are interested,please contact us by email
304 stainless steel is a general-purpose stainless steel with better rust and high-temperature resistance (up to 1000–1200°C) than 200-series, excellent corrosion and intergranular corrosion resistance, and good resistance to nitric acid (≤65% at boiling), alkalis, and most organic/inorganic acids. 304L is its low-carbon austenitic version (Cr ≥18%, Ni ≥8%, C ≤0.03), ideal for household and commercial applications due to excellent corrosion resistance, formability, and weldability by all fusion and resistance welding processes.
Grade 316 is an austenitic stainless steel with 2–3% molybdenum, which improves resistance to pitting, corrosion, and high-temperature exposure, making it particularly effective in acidic environments against acetic acid, hydrochloric acid, and other acids. 316L is its low-carbon version, also containing nickel and molybdenum; it resists sensitization (grain boundary carbide precipitation), is often used for large-gauge welded parts (over ~6 mm), and has higher creep, fracture stress, and tensile strength than chromium-nickel austenitic stainless steel at high temperature.
Type 201 stainless steel is an austenitic chromium-nickel-manganese stainless steel, which is developed to save nickel. Type 201 is a low-cost alternative to traditional Cr-Ni stainless steels such as 301 and 304. The nickel is replaced by added manganese and nitrogen. It cannot be hardened by heat treatment, but can reach high tensile strength by cold working. Type 201 is essentially non-magnetic in the annealed condition and becomes magnetic upon cold working. In many applications, the 201 type may replace the 301 type.
301 grade stainless steel is a common austenitic stainless steel with good corrosion resistance and high carbon content, and can be cold worked to various temperatures. Among stainless steels, 301 is the most easily strengthened steel by cold deformation. Cold deformation processing can improve the strength and hardness of steel, and retain sufficient plasticity and toughness. In addition, this steel has good rust resistance under atmospheric conditions, but its corrosion resistance in reducing media is poor, and its corrosion resistance in chemical media such as acid, alkali and salt is poor. Therefore, it is not recommended for corrosive environments.
310S is an austenitic stainless steel that combines excellent high temperature performance with good ductility and weldability. It is usually used for high temperature applications because its high chromium and nickel content provides solid corrosion resistance, excellent oxidation resistance and excellent strength at temperatures up to 2100 °F. Due to its high chromium and nickel content, it is superior to 304 or 309 stainless steel in most environments.
430 grade is a ferritic, straight chromium, non-hardenable grade that combines good corrosion resistance and formability characteristics with useful mechanical properties. Its resistance to nitric acid attack allows it to be used in specific chemical applications, but automotive trim and electrical components represent its largest areas of application.
305 stainless steel is an austenitic chromium-nickel stainless steel with a low work hardening rate. This low work hardening rate makes it suitable for many deep drawing applications. In order to minimize the earrings during the drawing process, the directionality introduced during the cold rolling process must be kept to a minimum.